The cathode is composed of mixed oxides of nickel, manganese and cobalt.
Each element plays a specific role. Nickel is the main player in increasing capacity (intercalation of lithium ions), manganese forms the skeleton that maintains the structure, and cobalt improves conductivity by facilitating charge transport.
The anode is usually made of graphite, in one of its industrial variants.
The first publication concerning a lithium-ion cell using an NMC cathode is attributed to Tsutomu Ohzuku and Yoshinari Makimura, from Osaka City University (Japan), in 2001.
South African chemist Michael Thackeray, from Argonne National Laboratory (USA), subsequently played a significant role in the development and industrialization of various forms of NMC chemistry. This was the culmination of many years of research on transition metal oxides, which began at Oxford University in the laboratory of B. Goodenough and notably led to the invention of manganese spinel.
In 2005, Milwaukee and Makita simultaneously launched their range of professional tools equipped with NMC lithium batteries as a replacement for the heavy and less efficient Ni-Cd.
NMC technology is particularly suited to applications that require high energy density and where safety can be perfectly controlled.
Examples:
NMC111: This is the historical, equimolar variant, with the most favorable (high) runaway temperature, at the expense of capacity (approx. 160 Ah/kg).
NMC532: Variants with more nickel are being developed to increase the capacity of NMC cells.
NMC622: This intermediate composition has a slightly better energy density compared to NMC111 but is less favorable in terms of safety with a slightly lower runaway temperature.
NMC811: The nickel-rich variant offers the highest energy density. However, it has the lowest thermal runaway temperature (approx. 200°C).
Parameter sets required for simulation models are available for different anode/cathode variants in the following publications: